Two blasting jobs can use the same abrasive and still finish very differently. The variable is grit size. Grain size sets how hard each particle hits, how much each pass removes, and what the surface looks like afterwards. Choosing it well means matching the size to the coating, the substrate and the finish the next step needs.
Coarse grain: faster cutting, deeper profile
Coarse sizes such as F24 and F36 carry more mass per particle, so each impact removes more coating or rust. They suit heavy scale and thick old paint, and preparation for thick coatings, where a deep anchor pattern helps the new coating grip. The trade-off is finish: a coarse grain leaves a rough profile that a thin coating may not cover evenly, and profile peaks can show through. Coarse grain also breaks down during use, so a cabinet running coarse grit accumulates finer material unless it is screened out.
Fine grain: control and finish
Fine sizes such as F120 and F220 hit lighter and remove less per pass, which makes them easier to control on thin sections, soft metals and parts where dimensions matter. They leave a smoother finish and a shallow profile suited to thin coatings and cleaning work where the surface should look uniform. The cost is speed: stripping a thick coating with fine grain takes more passes, and the fine dust it generates needs extraction that keeps cabinet visibility usable.
Profile depth and the next coating
Blasting is preparation, not the finished job, so the profile it leaves must fit what comes next. A coating specification often states the profile depth it needs: too shallow and the coating has little to grip; too deep and it must fill valleys it was not designed for, using more coating per square metre while peaks remain exposed. Before a production run, blast a test panel at the chosen size and measure the profile against the coating requirement rather than judging by eye. The grit size chart lists the F series sizes side by side, and the FEPA F vs P guide explains which grading series a blasting specification refers to.
Consumption, dust and reuse
Grain size also shapes running cost. Coarse grain tends to survive more impacts before breaking below usable size, while fine grain reaches dust size sooner, so the two sizes are consumed at different rates in the same cabinet. In a recycling system, screening separates reusable grain from dust and undersize; in a single-pass setup the spent grain is discarded. Either way, dust control matters: fine airborne particles reduce visibility in the cabinet, load the extraction filters and add to disposal volume.
Picking a starting size
Work back from the job: the coating or scale to remove, the substrate and its thickness, the finish the surface needs, and the profile the next coating asks for. A medium size such as F60 or F80 is a practical starting point for general cleaning and preparation; move coarser when removal is slow, move finer when the finish is too rough or thin parts are at risk. A short trial on a sample piece, at the pressure and nozzle distance the job will use, settles the choice faster than a specification sheet. The brown fused alumina F-grit range sets out the sizes commonly supplied for blasting work.